| Free Cutting Rephosphorized and Resulfurized Steels |
| Chemical Composition Ranges and Limits |
| SAE No. |
C |
Mn |
P |
S |
| 1212 |
.13 max |
.70/1.00 |
.07/.12 |
.16/.23 |
| 1213 |
.13 max |
.70/1.00 |
.07/.12 |
.24/.33 |
| 1215 |
.09 max |
.75/1.05 |
.04/.09 |
.26/.35 |
NOTE: 12XX grades are customarily furnished without specified silicon content because of adverse effect on machinability.